MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Toyobo GUR® 5113 UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Product Description: Melt processable UHMW-PE pellet grade. Some of the listed data have been determined from the virgin powder material.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183
Viscosity Number 1700 cm³/g17.0 dl/gIntrinsic; ISO 1628
 1900 cm³/g19.0 dl/gPE and PP; ISO 1628
Molecular Weight 3.70e+6 g/mol3.70e+6 g/molMargolies Equation
Melt Flow <= 0.10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
<= 0.10 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62
@Time 15.0 sec
62
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 37.0 MPa5370 psiISO 527-2/1B
Tensile Strength, Yield 22.0 MPa3190 psiISO 527-2/1B
Elongation at Break 430 %430 %Nominal; ISO 527-2/1B
Elongation at Yield 12 %12 %ISO 527-2/1B
Tensile Modulus 0.800 GPa116 ksiISO 527-1/1B
Charpy Impact, Notched 19.0 J/cm²90.4 ft-lb/in²Double 14° V-Notch; ISO 21304-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmIEC 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 80.0 °C176 °FISO 306/B50
 
Descriptive Properties
Elongational Stress17 psiF, 150/10, ISO 21304-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6292 / 310985

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.