MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® 6165 X Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded; Polycarbonate, Unreinforced, Flame Retardant

Material Notes: MVR (300 °C/1.2 kg) 28 cm³/10 min; flame retardant; UL 94V-0/1.2 mm; low viscosity; easy release; injection molding - melt temperature 280 - 320 °C; available in opaque colors only; LCD tv frame

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.640 g/ccpellets; ISO 60
Density 1.20 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.12 %ISO 62, 50% RH
Water Absorption at Saturation 0.30 %ISO 62
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmparallel/normal; b.o. ISO 2577
Linear Mold Shrinkage, Flow 0.0065 cm/cm
@Thickness 2.00 mm
60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 2.00 mm
60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 30 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 4800 N
@Temperature 23.0 °C
ISO 6603-2
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 65.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %Nominal, 50 mm/min; ISO 527-1,-2
 120 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 6.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2350 MPa1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Thickness 3.20 mm,
Temperature -30.0 °C
complete break; b.o. ISO 180-A
 15.0 kJ/m²
@Thickness 3.20 mm,
Temperature 23.0 °C
complete break; b.o. ISO 180-A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched 12.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
complete break; ISO 7391/b.o. ISO 179-1eA
 15.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
complete break; ISO 7391/b.o. ISO 179-1eA
Puncture Energy 45.0 J
@Temperature 23.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Comparative Tracking Index 125 VCTI M; Solution B; IEC 60112
 225 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-Kcross-flow; ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 136 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 124 °CISO 75-1,-2
Vicat Softening Point 143 °C
@Load 5.10 kg
50°C/h; ISO 306
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.20 mm
Flash Point 460 °CASTM D 1929
 530 °Cself ignition; ASTM D 1929
Oxygen Index 35 %Method A; ISO 4589-2
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection molding; ISO 294
Mold Temperature 80.0 °CInjection molding; ISO 294
Injection Velocity 200 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6265X Polycarbonate
Covestro Makrolon® 6255 Polycarbonate
Covestro Bayblend® FR3010 HF PC/ABS Blend
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade
Covestro Makrolon® 2467 Polycarbonate

PB09632 / 150764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.