MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Stycast® 2760 Two-Component Easy Mix Ratio Encapsulant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes:
Features and Typical Applications
Primarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, thermal and mechanical shock resistance, and thermal conductivity.

Emerson & Cuming 2760 Stycast® Two-Component Easy Mix Ratio Encapsulant
  • Mix Ratio by weight = 100:50
  • Good Chemical Resistance
  • Thermally Conductive
  • Filled
Cure Type: Room Temp or Heat Bonding Type: Epoxy/Polyurethane

The Stycast® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/cc
Viscosity 18000 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.0
@Frequency 1e+6 Hz
Dielectric Strength 450 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 122 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.600 W/m-K
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time >= 2.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 2072 Two-Component Easy Mix Ratio Encapsulant
Henkel Loctite® Stycast® 2851FT One-Component Thermally Conductive Encapsulant
Trelleborg Emerson & Cuming Stycast® E-151-8 One-Component Epoxy Flexible Encapsulant
Trelleborg Emerson & Cuming Stycast® E-1000 One-Component Epoxy Low Stress Encapsulant
Trelleborg Emerson & Cuming Stycast® 2754 Two-Component Epoxy Flexible Low-Stress Encapsulant

PEMERS30 / 35722

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.