MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Hysol Benzoxazine 99120 Infusion Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: One-part Infusion resin for VARTM processing. Moderate viscosity, very high toughness with good hot wet properties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 23.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 97.0 MPa
Elongation at Break 4.6 %
Tensile Modulus 3700 MPa
Flexural Modulus 3500 MPa
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Glass Transition Temp, Tg 147 °CWet - 72 Hour Boil
 180 °CDry
 
Processing PropertiesOriginal ValueComments
Cure Time 1.50 hour
@Temperature 180 °C
Pot Life 180 day
 
Descriptive Properties
ConsistencyModerate Viscosity
Form1 part
Fracture Toughness (J/m2)471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol Benzoxazine 99110 Infusion Resin
Solvay CYCOM® 7714A Epoxy - Unidirectional Carbon Tape and Roving Composite
Solvay CYCOM® 977-20 Resin System with PRIFORM™ Technology
Henkel Hysol Benzoxazine 99900 Infusion Resin Binder
Huntsman Tactix 742 Multifunctional Resin

PHENK828 / 146833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.