MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BASF 3D Ultrafuse® HiPS Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Components: High impact Polystyrene based filament for Fused Filament Fabrication.

Product Description: Ultrafuse HiPS is a high-quality engineering thermoplastic, which is well known in the 3D-printing industry as a support material for ABS. But this material has additional properties to offer like good impact resistance, good dimensional stability, and easy post-processing. HiPS is a great material to use as a support for ABS because there is a good compatibility between the two materials, and HiPS is an easy breakaway support. Now you have the opportunity to create ABS models with complex geometry. Our HiPS is easy to post process with glue or with sanding paper.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.023 g/cc0.03696 lb/in³Printed Part; ISO 1183-1
Melt Flow 29.3 g/10 min
@Load 2.16 kg,
Temperature 260 °C
29.3 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.7 MPa1990 psiZX: Upright; ISO 527
 18.4 MPa2670 psiXY: Flat; ISO 527
Elongation at Break 1.3 %1.3 %ZX: Upright; ISO 527
 1.4 %1.4 %XY: Flat; ISO 527
Modulus of Elasticity 1.588 GPa230.3 ksiYoung's, XY: Flat; ISO 527
 1.603 GPa232.5 ksiYoung's, ZX: Upright; ISO 527
Flexural Strength 26.8 MPa3890 psiZX: Upright; ISO 178
 31.8 MPa4610 psiXY: Flat; ISO 178
 32.2 MPa4670 psiXZ: On its edge; ISO 178
Flexural Modulus 1.227 GPa178.0 ksiZX: Upright; ISO 178
 1.526 GPa221.3 ksiXZ: On its edge; ISO 178
 1.635 GPa237.1 ksiXY: Flat; ISO 178
Flexural Strain at Break 4.6 %4.6 %ZX: Upright; ISO 178
 5.2 %5.2 %XZ: On its edge; ISO 178
 5.4 %5.4 %XY: Flat; ISO 178
Izod Impact, Notched (ISO) 4.80 kJ/m²2.28 ft-lb/in²ZX: Upright; ISO 180
 6.90 kJ/m²3.28 ft-lb/in²XY: Flat; ISO 180
 7.10 kJ/m²3.38 ft-lb/in²XZ: On its edge; ISO 180
Izod Impact, Unnotched (ISO) 9.10 kJ/m²4.33 ft-lb/in²ZX: Upright; ISO 180
 35.0 kJ/m²16.7 ft-lb/in²XY: Flat; ISO 180
 57.1 kJ/m²27.2 ft-lb/in²XZ: On its edge; ISO 180
Charpy Impact Unnotched 0.860 J/cm²4.09 ft-lb/in²ZX: Upright; ISO 179
 3.60 J/cm²17.1 ft-lb/in²XY: Flat; ISO 179
 5.76 J/cm²27.4 ft-lb/in²XZ: On its edge; ISO 179
Charpy Impact, Notched 0.410 J/cm²1.95 ft-lb/in²ZX: Upright; ISO 179
 0.650 J/cm²3.09 ft-lb/in²XY: Flat; ISO 179
 0.660 J/cm²3.14 ft-lb/in²XZ: On its edge; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °FISO 75-2
Glass Transition Temp, Tg 99.0 °C210 °FISO 11357-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 120 °C212 - 248 °FBed, Bed Material: Spray
Nozzle Temperature 240 - 260 °C464 - 500 °F
Drying Temperature 60.0 °C140 °Fin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour4.00 - 16.0 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed40-80 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF3D020 / 312261

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.