MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultramid® STAR S 218 V30 NATURAL Nylon 6, 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Product Description: Ultramid® STAR S 218 V30 NATURAL is based on a patented high flow polyamide 6 resin, heat stabilized, reinforced with 30% of glass fiber, for injection molding. Due to its outstanding flow characteristics, this grade provides a significant productivity improvement and allows more freedom in mold and part design versus a standard polyamide solutions.

Availability: Africa & Middle East; Asia Pacific; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer

Features: Good Dimensional Stability; Good Mold Release; Heat Stabilized – Inorganic; High Flow; Outstanding Surface Finish

Uses: Consumer Applications; Furniture; General Purpose; Industrial Applications

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Water Absorption 2.0 %2.0 %Equilibrium, 50% RH; ISO 62
 0.95 %
@Time 86400 sec
0.95 %
@Time 24.0 hour
ISO 62
Maximum Moisture Content 0.200.20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psiISO 527-2
Elongation at Break 3.0 %3.0 %ISO 527-2
Tensile Modulus 10.0 GPa1450 ksiISO 527-1
Flexural Strength 250 MPa36300 psiISO 178
 255 MPa37000 psiASTM D790
Flexural Modulus 8.62 GPa1250 ksiASTM D790
 9.03 GPa1310 ksiISO 178
Izod Impact, Notched (ISO) 3.99 kJ/m²1.90 ft-lb/in²ASTM D256
 12.0 kJ/m²
@Temperature 22.8 °C
5.70 ft-lb/in²
@Temperature 73.0 °F
ISO 180/A
 15.7 kJ/m²
@Temperature -30.0 °C
7.50 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched 6.93 J/cm²33.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.70 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FUnannealed; ASTM D648
 205 °C401 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 3.30 mm
HB
@Thickness 0.130 in
IEC 60695-11-10,-20
Glow Wire Flammability Index 649 °C
@Thickness 1.52 mm
1200 °F
@Thickness 0.0600 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 235 °C446 - 455 °F
Middle Barrel Temperature 235 - 240 °C455 - 464 °F
Front Barrel Temperature 240 - 245 °C464 - 473 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2042 / 310735

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.