MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Devcon® FasMetal™
Categories: Polymer; Thermoset; Epoxy

Material Notes: A high-performance, fast-curing 100% solids epoxy for emergency repairs to stainless steel, equipment that needs good chemical resistance. Uses: Repair breakers and transformers in an emergency; patch holes and leaks in coal fuel lines; repair cracks in housing and pipes; rebuild keyways and treads. Features: Can be applied in temperatures as low as 40°F, Full cure in 6 hours, Easy to use 1:1 formula, Sets up in 5 minutes.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.69 g/cc1.69 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ASTM D2240
Modulus of Elasticity 5.86 GPa850 ksi
Flexural Strength 53.1 MPa7700 psiASTM D790
Compressive Strength 87.6 MPa12700 psiASTM D695
Shear Strength 13.8 MPa2000 psiASTM D1002
Adhesive Bond Strength 13.8 MPa2000 psiAdhesive Tensile Shear; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 18.618.6ASTM D150
Dielectric Strength 14.6 kV/mm371 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 57.6 µm/m-°C32.0 µin/in-°FASTM D696
Thermal Conductivity 0.854 W/m-K5.93 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 121 °C250 °FTemperature Resistance - Dry
Shrinkage 0.93 %0.93 %Linear During cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 24.0 °C
1.00 hour
@Temperature 75.2 °F
Functional cure
 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
As Tested
Pot Life 4.00 min
@Temperature 23.9 °C
4.00 min
@Temperature 75.0 °F
3/4 lb. mass
 
Descriptive Properties
Chemical/Solvent Resistance1,1,1-Trichloroethane: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Ammonium Hydroxide 20%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting oil: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methylene Chloride: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Mineral Spirits: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 40%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Chloride Brine: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%:: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%:: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite:: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10% : fair30 day immersion at 75°F. Sample cured 7 days at RT
 Trisodium Phosphate: fair30 day immersion at 75°F. Sample cured 7 days at RT
ColorGray
Coverage69 in²/lbCured. @ 1/4"
Mix Ratio by volume1:1
Mix Ratio by weight1.07:1
Recoat Time30 min
Specific Volume (in.³/lb)17.2Cured
ViscosityNon-sag Putty. Mixed.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9203 / 239713

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.