System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Geon® Performance Solutions 83520 Fiberloc PVC; 20% Glass Fiber Reinforced
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
;
PVC, 20% Glass Fiber Reinforced
Material Notes:
Medium Impact, High Flow. Weatherable, high flow, 20% glass fiber reinforced compound for injection molding or extrusion applications.
Data provided by the manufacturer, The Geon Company.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.52
g/cc
ASTM D792
Linear Mold Shrinkage
0.00
-
0.015
cm/cm
ASTM D955
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
108
ASTM D785
Hardness, Shore D
83
ASTM D2240
Tensile Strength, Ultimate
66.0
MPa
at 5 cm/min. ASTM D638
Elongation at Break
2.0 %
at 5 cm/min. ASTM D638
Modulus of Elasticity
6.551
GPa
at 5 cm/min. ASTM D638
Flexural Yield Strength
103
MPa
ASTM D790
Flexural Modulus
6.206
GPa
ASTM D790
Poissons Ratio
0.42
ASTM E132
Shear Modulus
2.31
GPa
Calculated
Izod Impact, Notched
0.600
J/cm
@Diameter 3.20 mm
bar; ASTM D256
Izod Impact, Unnotched
3.20
J/cm
@Diameter 3.20 mm
bar; ASTM D256
Thermal Properties
Original Value
Comments
CTE, linear
27.1
µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)
76.0
°C
Annealed; 6.4 cm (2.5 in.) bars; ASTM D648
Flammability, UL94
V-0
May vary with color or thickness
Processing Properties
Original Value
Comments
Melt Temperature
195
-
205
°C
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Geon® Performance Solutions 83530 Fiberloc PVC; 30% Glass Fiber Reinforced
Geon® Performance Solutions 87447 Molding PVC
Teknor Apex APEX® SIC 3705 Rigid Polyvinyl Chloride
Geon® Performance Solutions 82530 Fiberloc PVC; 30% Glass Fiber Reinforced
Geon® Performance Solutions 82520 Fiberloc PVC; 20% Glass Fiber Reinforced
PVIGB9 / 71854
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.