MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huber Martoxid® MPS Calcined Aluminum Oxide
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Martoxid® MPS calcined aluminum oxide is a fine-grained, very soft aluminum oxide for the production of high brilliance polishing agents for a variety of ferrous and nonferrous metals, and for the fine grinding of plastics and lacquers.

CAS No.: 1344-28-1

EC/EINECS No.: 215-691-6

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.950 g/cc0.0343 lb/in³
Particle Size <= 45 µm<= 45 µm<20 percent, Screening
 45 - 63 µm45 - 63 µm4-20 percent, Screening
 63 - 106 µm63 - 106 µm40-70 percent, Screening
 >= 106 µm>= 106 µm10-50 percent, Screening
Specific Surface Area 3.0 - 6.0 m²/g3.0 - 6.0 m²/gBET
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 70 %>= 70 %a-Al2O3
CaO 0.020 %0.020 %
Fe2O3 0.020 %0.020 %
Loss on Ignition(%) <= 0.20 %<= 0.20 %
Na2O <= 0.10 %<= 0.10 %total
SiO2 0.040 %0.040 %
 
Descriptive Properties
Al(OH)3 (%)99.8
FunctionalityInert filler
Functionality: Mechanical hardnessAbrasive
Functionality: Optical effectsTitanium Dioxide (TiO2) Extender
Market/Application: IndustrialCeramics
Market/Application: TransportationPolishing
Primary Crystal1 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER812 / 300918

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.