MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin ENG265 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ ENG265 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This material is suitable for profile extrusion and exhibits very good hydrolytic stability, low moisture absorption, good dimensional stability. NORYL ENG265 resin is an excellent candidate for a variety of profile extrusion applications. *See ENG265F resin for NSF 61 certification.

Features: Hydrolytic Stability,Low Creep Sensitivity,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Extrusion
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 280 °C
8.0 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 8.5 g/10 min
@Load 5.00 kg,
Temperature 280 °C
8.5 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength at Break 50.0 MPa7250 psiASTM D638
 50.0 MPa7250 psiISO 527
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
 56.0 MPa8120 psi50 mm/min; ASTM D638
Elongation at Break 27 %27 %ISO 527
 28 %28 %50 mm/min; ASTM D638
Elongation at Yield 3.1 %3.1 %ISO 527
 3.3 %3.3 %ASTM D638
Tensile Modulus 2.40 GPa348 ksi5 mm/min; ASTM D638
 2.55 GPa370 ksi1 mm/min; ISO 527
Flexural Strength 88.0 MPa12800 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
 89.0 MPa12900 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 95.0 MPa13800 psiISO 178
Flexural Modulus 2.45 GPa355 ksi2.6 mm/min, 100 mm span; ASTM D790
 2.50 GPa363 ksiISO 178
 2.55 GPa370 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 186 J137 ft-lbASTM D256
 114 J
@Temperature -30.0 °C
84.1 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179/2C
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/2C
Gardner Impact  5.00 J
@Temperature -40.0 °C
3.69 ft-lb
@Temperature -40.0 °F
ASTM D3029
 25.0 J
@Temperature -30.0 °C
18.4 ft-lb
@Temperature -22.0 °F
ASTM D3029
Dart Drop, Total Energy 39.0 J28.8 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.65
@Frequency 50.0 - 60.0 Hz
2.65
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm
@Thickness 3.20 mm
500 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor 0.00040
@Frequency 50.0 - 60.0 Hz
0.00040
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=6.00 mm
7.0 - 15 sec
@Thickness >=0.236 in
UL 746A
 30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=6.00 mm
0.00 - 15 arcs
@Thickness >=0.236 in
UL 746A
 >= 120 arcs
@Thickness >=1.50 mm
>= 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 59.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
33.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi)  132 °C
@Thickness 3.20 mm
270 °F
@Thickness 0.126 in
unannealed; ASTM D648
 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  118 °C
@Thickness 3.20 mm
244 °F
@Thickness 0.126 in
unannealed; ASTM D648
 126 °C
@Thickness 6.40 mm
259 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 137 °C279 °FRate B/50; ISO 306
 141 °C286 °FRate B/120; ISO 306
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 1 205 °C401 °FExtrusion
Zone 2 205 °C401 °FExtrusion
Zone 3 225 °C437 °FExtrusion
Zone 4 225 °C437 °FExtrusion
Adapter Temperature 250 °C482 °FExtrusion
Die Temperature 250 °C482 °FExtrusion
Melt Temperature 225 - 255 °C437 - 491 °FExtrusion
Drying Temperature 105 - 115 °C221 - 239 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion
 8.00 hour8.00 hourCumulative; Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82280 / 290227

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.