MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik Multilayer Tubing 8000 series
Categories: Other Engineering Material

Material Notes: Three-Layer coolant lines made from VESTAMID®. The multilayer tubing system (MLT) 8000 is an automotive industry proven 3-layer system for thermal management systems. With an outer layer of VESTAMID® polyamide 12 and a special polypropylene inner layer the system offers high hydrolysis resistance against coolant liquids and urea solutions, good cold impact performance and significantly weight savings compared to less innovative concepts (metal/ rubber hoses).
Industrial Sector: Automotive and Mobility
Processing: Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Hydrolysis / hot water
Electrical: Insulating
Conformity: Automotive
Applications: Tube and hose , Refrigeration
Processing: Thermoforming, Pipe/Tube extrusion, Coextrusion (MLT)
Features: Lightweight
Chemical Resistance: Hydrolytically stable

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7808 / 324940

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.