MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Multibase Multi-Flex® TPO D 5302 E MB
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Data provided by Multibase.

Key Words: Thermoplastic Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955-89
Melt Flow 1.0 g/10 min1.0 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 535310 sec; ASTM D-2240-95
Tensile Strength, Ultimate 22.4 MPa3250 psiASTM D638-95
Elongation at Break 630 %630 %ASTM D638-95
Flexural Strength 17.4 MPa2520 psiASTM D790-95
Flexural Modulus, 1% Secant 690 MPa100000 psiASTM D-790-95
Izod Impact, Notched NBNBASTM D-256-93a
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FASTM D648-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Flex® TPE A 3299 NAT
Multibase Multi-Flex® TPE A 3005 F
Multibase Multi-Flex® TPE A 7204 LC BLK

PLA221 / 49618

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.