MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Solvay AeroPaste® 1006 Adhesive
Categories: Polymer; Adhesive

Material Notes: AeroPaste® 1006 is a two-part, low-temperature-curing paste adhesive designed for out-of-autoclave structural bonding and rapid assembly applications. AeroPaste 1006 paste adhesive provides high strength, high toughness and excellent hot/wet properties with flexible curing schedules and ease of use.

Features & Benefits:

  • Service temperature of 250°F (121°C) dry and 180°F (82°C) hot/wet
  • Good combination of shear and peel properties
  • Slump resistant and designed for automated dispensing
  • High glue line thickness tolerance
Suggested Applications:
  • Structural bonding of metals and composites
  • Repair applications
Note 1: Bond Gap Tolerance Using Glass Beads and ShimWires at 80 mils-AeroPaste 1006 out-of-autoclave cured at 200°F (93°C) for 2 hours on PAA-treated bare 2024-T3 aluminum with BR® 127 primer

Note 2: AeroPaste 1006, 0.06 psf (GLT = 10 mil) on PAA-treated bare 2024-T3 aluminum with BR 127 primer

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³Part B
 1.05 g/cc0.0379 lb/in³Mixed
 1.05 g/cc0.0379 lb/in³Cured
 1.10 g/cc0.0397 lb/in³Part A
Viscosity 200 cP200 cPPart B
 400 cP400 cPInitial Mixed
 810 cP810 cPPart A
Storage Temperature 24.0 °C75.2 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  11.35 MPa
@Temperature 121 °C
1646 psi
@Temperature 250 °F
Blister, Note 2, Cure cycle 71°C for 6 hrs
 16.50 MPa
@Temperature 121 °C
2393 psi
@Temperature 250 °F
Blister, Note 2, Cure cycle 82°C for 4 hrs
 17.7 MPa
@Temperature 121 °C
2560 psi
@Temperature 250 °F
Blister, Cure cycle 93°C for 2 hrs
 18.40 MPa
@Temperature 121 °C
2668 psi
@Temperature 250 °F
Blister, Note 2, Cure cycle 93°C for 2 hrs
 25.19 MPa
@Temperature 82.0 °C
3654 psi
@Temperature 180 °F
Blister, Note 2, Cure cycle 71°C for 6 hrs
 25.22 MPa
@Temperature 82.0 °C
3658 psi
@Temperature 180 °F
Blister, Note 2, Cure cycle 93°C for 2 hrs
 25.92 MPa
@Temperature 82.0 °C
3759 psi
@Temperature 180 °F
Blister, Cure cycle 93°C for 2 hrs
 26.23 MPa
@Temperature 82.0 °C
3804 psi
@Temperature 180 °F
Blister, Note 2, Cure cycle 82°C for 4 hrs
 34.44 MPa
@Temperature 24.0 °C
4995 psi
@Temperature 75.2 °F
Blister, Note 2, Cure cycle 71°C for 6 hrs
 35.20 MPa
@Temperature 24.0 °C
5105 psi
@Temperature 75.2 °F
Blister, Cure cycle 93°C for 2 hrs
 35.87 MPa
@Temperature 24.0 °C
5202 psi
@Temperature 75.2 °F
Blister, Note 2, Cure cycle 93°C for 2 hrs
 35.91 MPa
@Temperature 24.0 °C
5208 psi
@Temperature 75.2 °F
Blister, Note 2, Cure cycle 82°C for 4 hrs
 8.998 MPa
@Thickness 1.02 mm,
Temperature 121 °C
1305 psi
@Thickness 0.0400 in,
Temperature 250 °F
Blister, Note 1
 10.49 MPa
@Thickness 2.03 mm,
Temperature 121 °C
1521 psi
@Thickness 0.0800 in,
Temperature 250 °F
Blister, Note 1
 12.39 MPa
@Thickness 0.508 mm,
Temperature 121 °C
1797 psi
@Thickness 0.0200 in,
Temperature 250 °F
Blister, Note 1
 18.39 MPa
@Thickness 2.03 mm,
Temperature 24.0 °C
2667 psi
@Thickness 0.0800 in,
Temperature 75.2 °F
Blister, Note 1
 18.40 MPa
@Thickness 0.254 mm,
Temperature 121 °C
2668 psi
@Thickness 0.0100 in,
Temperature 250 °F
Blister, Note 1
 18.60 MPa
@Thickness 0.508 mm,
Temperature 82.0 °C
2697 psi
@Thickness 0.0200 in,
Temperature 180 °F
Blister, Note 1
 19.59 MPa
@Thickness 2.03 mm,
Temperature 82.0 °C
2842 psi
@Thickness 0.0800 in,
Temperature 180 °F
Blister, Note 1
 19.75 MPa
@Thickness 1.02 mm,
Temperature 82.0 °C
2865 psi
@Thickness 0.0400 in,
Temperature 180 °F
Blister, Note 1
 19.80 MPa
@Thickness 1.02 mm,
Temperature 24.0 °C
2872 psi
@Thickness 0.0400 in,
Temperature 75.2 °F
Blister, Note 1
 25.79 MPa
@Thickness 0.254 mm,
Temperature 82.0 °C
3741 psi
@Thickness 0.0100 in,
Temperature 180 °F
Blister, Note 1
 29.68 MPa
@Thickness 0.508 mm,
Temperature 24.0 °C
4304 psi
@Thickness 0.0200 in,
Temperature 75.2 °F
Blister, Note 1
 35.87 MPa
@Thickness 0.254 mm,
Temperature 24.0 °C
5202 psi
@Thickness 0.0100 in,
Temperature 75.2 °F
Blister, Note 1
Peel Strength 8.77 kN/m50.0 pliBell, Note 2, Cure cycle 93°C for 2 hrs
 9.64 kN/m55.0 pliBell, Note 2, Cure cycle 93°C for 2 hrs
 11.2 kN/m64.0 pliBell , Note 2, Cure cycle 82°C for 4 hrs
 11.7 kN/m67.0 pliBell, Note 2, Cure cycle 93°C for 2 hrs
 14.0 kN/m80.0 pliBell, Note 2, Cure cycle 71°C for 6 hrs
 6.31 kN/m
@Thickness 1.02 mm,
Temperature 82.0 °C
36.0 pli
@Thickness 0.0400 in,
Temperature 180 °F
FR Peel, Note 1
 7.54 kN/m
@Thickness 1.02 mm,
Temperature 24.0 °C
43.0 pli
@Thickness 0.0400 in,
Temperature 75.2 °F
FR Peel, Note 1
 8.41 kN/m
@Thickness 0.508 mm,
Temperature 24.0 °C
48.0 pli
@Thickness 0.0200 in,
Temperature 75.2 °F
FR Peel, Note 1
 9.47 kN/m
@Thickness 0.508 mm,
Temperature 121 °C
54.0 pli
@Thickness 0.0200 in,
Temperature 250 °F
FR Peel, Note 1
 9.64 kN/m
@Thickness 0.254 mm,
Temperature 24.0 °C
55.0 pli
@Thickness 0.0100 in,
Temperature 75.2 °F
FR Peel, Note 1
 10.3 kN/m
@Thickness 1.02 mm,
Temperature 121 °C
59.0 pli
@Thickness 0.0400 in,
Temperature 250 °F
FR Peel, Note 1
 17.9 kN/m
@Thickness 0.508 mm,
Temperature 82.0 °C
102 pli
@Thickness 0.0200 in,
Temperature 180 °F
FR Peel, Note 1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °FWet
 121 °C250 °FDry
Glass Transition Temp, Tg  120 - 122 °C
@Treatment Temp. 93.3 °C,
Time 7200 sec
248 - 252 °F
@Treatment Temp. 200 °F,
Time 2.00 hour
Wet
 122 - 124 °C
@Treatment Temp. 93.3 °C,
Time 7200 sec
252 - 255 °F
@Treatment Temp. 200 °F,
Time 2.00 hour
Dry
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorDark BluePart A
 GreenMixed
 GreenCured
 YellowPart B
Mix Ratio100:45by weight
 2:1by volume
Vertical Slump0.140.375" thick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCYTED001 / 180303

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.