MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell CirculenRecover C14 LD2420F Plus LDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: CirculenRenew C14 LD2420 F Plus is part of the Circulen© product family of circular and sustainable solutions. CirculenRenew C14 polymer reduces the carbon footprint as it replaces fossil feedstock through using renewable raw materials made from bio-based waste and residue oils. The renewable content of CirculenRenew C14 is measured by an accredited third party laboratory and stated as a parameter on the Certificate of Analysis (CoA). CirculenRenew C14 LD2420 F Plus is a drop-in solution and therefore doesn’t require any adaptation of the existing processing equipment. CirculenRenew C14 LD2420 F Plus is a non-additivated, low density polyethylene. This grade is characterized by a very low gel level. Typical customer applications are surface protection films or other higher value film applications where a very low gel content is required . It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications.

Status: Commercial - Active

Availability: Africa-Middle East; Asia-Pacific; Europe

Application: Bags & Pouches; Food Packaging Film; Hygiene Film; Liner Film; Shrink Film; Surface Protection Film

Market: Flexible Packaging

Processing Method: Blown Film

Attribute: General Purpose; Good Heat Seal; Good Melt Strength; Good Optical Properties; Good Processability; Low Gel

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ISO 1183-1
Melt Flow 0.750 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.750 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 11.0 MPa1600 psiISO 527-1, -2
Film Elongation at Break, MD 300 %300 %ISO 527-1, -3
Film Elongation at Break, TD 600 %600 %ISO 527-1, -3
Tensile Modulus 0.260 GPa37.7 ksiISO 527-1, -2
Coefficient of Friction >= 0.800>= 0.800ISO 8295
Dart Drop Test 150 g0.331 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 26.0 MPa3770 psiISO 527-1, -3
Film Tensile Strength at Break, TD 24.0 MPa3480 psiISO 527-1, -3
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °FPeak; ISO 11357-3
Vicat Softening Point 96.0 °C205 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 8.00 %
@Thickness 0.0500 mm
<= 8.00 %
@Thickness 0.00197 in
ASTM D1003
Gloss >= 40.0 %>= 40.0 %20°; ASTM D2457
 >= 90.0 %>= 90.0 %60°; ASTM D2457
 
Descriptive Properties
Failure Energy5.5 J/mmDIN 53373

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9080 / 324015

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.