MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Trinseo PULSE™ 830 ABS + Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.

PULSE 830 Engineering resin has been used in automotive instrument panel and interior trim applications.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM Data
Melt Density 0.962 g/cc0.0348 lb/in³
Water Absorption 0.15 %0.15 %
Moisture Absorption at Equilibrium 0.32 %0.32 %Humidity Absorption
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/in
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115
Tensile Strength, Ultimate 44.8 MPa6500 psiASTM Data
Tensile Strength, Yield 53.1 MPa7700 psiASTM Data
Elongation at Break 125 %125 %ASTM Data
Elongation at Yield 4.0 %4.0 %ISO Data
Tensile Modulus 2.30 GPa334 ksiISO Data.
Izod Impact, Notched 6.41 J/cm12.0 ft-lb/inASTM Data
 5.34 J/cm
@Temperature -50.0 °C
10.0 ft-lb/in
@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NBNBISO Data
 NBNBISO Data, Low Temp
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO Data, Low Temp
 6.60 J/cm²31.4 ft-lb/in²ISO Data
Instrumented Impact Total Energy  56.5 J
@Temperature 23.0 °C
41.7 ft-lb
@Temperature 73.4 °F
 62.2 J
@Temperature -30.0 °C
45.9 ft-lb
@Temperature -22.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 73.8 µm/m-°C
@Temperature 20.0 °C
41.0 µin/in-°F
@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 1.93 J/g-°C0.461 BTU/lb-°F
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FUnannealed; ASTM Data
 121 °C250 °Fannealed; ASTM Data

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo PULSE™ 930 ABS + Polycarbonate
Trinseo PULSE™ 710 ABS + Polycarbonate
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Trinseo MAGNUM™ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo PULSE™ 600 ABS + Polycarbonate

PZZDW129 / 34360

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.