MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP121AO Thermally Conductive, Dimensionally Stable Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced; Epoxy, High Temperature

Material Notes: Key Features:
  • Thermally conductive
  • Electrically insulative
  • Very long open time
  • Excellent temperature resistance
  • Medium viscosity liquid for potting applications
  • Outstanding dimensional stability
Product Description: Master Bond EP121AO is a two component, high performance epoxy resin system featuring top notch temperature resistance, impressive thermal conductivity, superior electrical insulation properties and outstanding dimensional stability. It has an easy to use 100:80 mix ratio by weight. After mixing EP121AO is a lower viscosity epoxy with wonderful flow properties for coating, sealing, potting and encapsulation applications. Adhesion to metals, composites, glass, ceramics and many rubbers and plastics is first rate. As mentioned previously its salient features include prominent thermal conductivity, reliable electrical insulation properties and striking dimensional stability. The service temperature range is -60°F to +500°F. EP121AO features an extremely long open time of 1-2 days but requires oven curing. A typical cure schedule is 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F, although, a number of variations are possible. It also should be noted that EP121AO has exceptionally low exotherm upon curing and is an excellent fit for larger sized encapsulation or potting applications. EP121AO is most commonly used in electronics as a potting and encapsulation material when the combination of properties mentioned above is desirable.

Product Advantages:

  • Medium viscosity liquid ideally suited for potting applications
  • Superb heat resistance
  • Exceptional physical strength properties and dimensional stability
  • High thermal conductivity and excellent electrical insulation properties
  • Good adhesion to a wide range of substrates
  • Very low coefficient of expansion
  • Exceptionally long working life at room temperature

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 35000 - 75000 cPPart B
 55000 - 95000 cPmixed
 100000 - 160000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85 - 90
Tensile Strength 9000 - 10000 psi
Elongation at Break 2.0 - 5.0 %
Tensile Modulus 600000 - 650000 psi
Compressive Strength 24000 - 26000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 3.00e+11 ohm-cm
@Temperature 150 °C
 >= 3.00e+12 ohm-cm
@Temperature 100 °C
 >= 3.00e+14 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 4.3
@Frequency 60 Hz
Dissipation Factor 0.31
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 - 21.0 µm/m-°C
Thermal Conductivity 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 121 °C
followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F
Working Life 720 - 1440 minAfter mixing, 100 g batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio100:80 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP113 Two Component Epoxy
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy
Aremco Aremco-Bond™ 2340 High Temperature Epoxide Potting Compound
Master Bond EP36AO One Part, Thermally Conductive, Heat Resistant Epoxy
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy

PMASTM911 / 185504

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.