MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Krytox® 1506XP Vacuum Pump Fluid with Antirust Protection
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox® VPF fluids are now available with antirust protection. The new fluids are called 1506XP, 1514XP, 1525XP, and 1531XP. They have all of the same properties of the standard fluids listed above. Krytox® XP VPF oils contain a soluble additive to prevent rust. This new patented additive enhances the performance of Krytox® VPF fluids, giving them improved performance properties. The long-term antirust properties repel moisture, providing extra protection from corrosion of metal parts and bearing surfaces. While Krytox® VPF fluids are inert and nonreactive to all elastomers, plastics, and metals, the soluble additives in the XP products are new and have not been tested with all materials. It is possible that some reactivity and damage could occur to some materials. Initial testing has shown no problems with Teflon®, Kalrex®, Viton®, nitrile, and silicone rubbers. There is some reactivity of the additive with copper, but it is less with brass. These additives could have degradation of performance at elevated temperatures over 175°C (347°F) over a long period of time.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.54 g/cc
@Temperature 200 °C
0.0556 lb/in³
@Temperature 392 °F
 1.73 g/cc
@Temperature 100 °C
0.0625 lb/in³
@Temperature 212 °F
 1.82 g/cc
@Temperature 50.0 °C
0.0658 lb/in³
@Temperature 122 °F
 1.88 g/cc
@Temperature 20.0 °C
0.0679 lb/in³
@Temperature 68.0 °F
Kinematic Viscosity  1.2 cSt
@Temperature 200 °C
1.2 cSt
@Temperature 392 °F
ASTM D445
 62 cSt
@Temperature 20.0 °C
62 cSt
@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 16 cSt16 cSt50°C; ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.4 cSt4.4 cStASTM D445
Molecular Weight 2400 g/mol2400 g/molNMR
Vapor Pressure Test 4.00e-7 torr4.00e-7 torr20°C; Knudsen
 0.0000100 torr0.0000100 torr50°C; Knudsen
 0.00100 torr0.00100 torr100°C; Knudsen
 0.500 torr0.500 torr200°C; Knudsen
Evaporation Loss 6.0 %6.0 %Volatility; 22 hr; 149°C; ASTM D792
 35 %35 %Volatility; 22 hr; 204°C; ASTM D792
 7.3 %
@Temperature 121 °C,
Time 79200 sec
7.3 %
@Temperature 250 °F,
Time 22.0 hour
Volatility; ASTM D2595
Surface Tension 17 dynes/cm17 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 37.7 J/g
@Temperature 150 - 250 °C
16.2 BTU/lb
@Temperature 302 - 482 °F
Knudsen
Distillation Temperature 160 - 220 °C320 - 428 °FDistillation Range at 0.4 torr
Pour Point -60.0 °C-76.0 °FASTM D97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Krytox® NRT 8906 PFPE Lubricant
Chemours Krytox® 1645 Vacuum Service Fluid
Chemours Krytox® 16256 Vacuum Pump Fluid
Chemours Krytox® 1531XP Vacuum Pump Fluid with Antirust Protection
Chemours Krytox® 1531 Vacuum Pump Fluid

WDUPK12 / 75372

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.