Sequel 1514-UV RXF AB thermoplastic polyolefin material exhibits significantly greater mar resistance than conventional TPOs. Sequel 1514-UV RXF AB polyolefin is typically used for automotive applications that demand low warpage and low CLTE, along with excellent scratch and mar resistance. Applications: Automotive Parts, Exterior Automotive ApplicationsInformation provided by LyondellBasell. |