MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling SUSTAMID® 66 PA 66/Extruded Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes:
  • Good dimensional stability
  • Very good sliding properties
  • High abrasion resistance
Product applications:
  • Mechanical engineering
  • Aircraft construction
  • Electrical industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 1.0 %
@Time 86400 sec
ASTM D570
Water Absorption at Saturation 8.5 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Hardness, Rockwell R 121ASTM D785
Hardness, Shore D 80ASTM D2240
Tensile Strength, Yield 12000 psiASTM D638
Elongation at Break 40 %ASTM D638
Tensile Modulus 400000 psiASTM D638
Flexural Strength 15000 psiASTM D790
Flexural Modulus 420000 psiASTM D790
Compressive Strength 12500 psiASTM D695
Shear Strength 10000 psiASTM D732
Izod Impact, Notched 0.600 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.25
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.8 kV/mmASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µin/in-°FASTM D696
Thermal Conductivity 1.70 BTU-in/hr-ft²-°F
Melting Point 500 °FASTM D3418
Maximum Service Temperature, Air 220 °F
Deflection Temperature at 0.46 MPa (66 psi) 390 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black
EPICHEM PA 66 Polyamide 66
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
EPICHEM Epinyl PA 66 Polyamide 66
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned

PROCH9036 / 232739

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.