MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Inov Chem Donpipe 301 Water base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: This product is a type of blend polyols with water as foaming agent, which is specially researched for rigid PUF to produce thermal insulation pipes. It is widely used in steam pipes, liquefied nature gas running pipes, oil pipes and other fields. The characteristics are as follows:

(1) good flowability, by regulating formula to suit different pipe diameters.

(2) high temperature-resistance performance, long standing in 150?

(3) excellent low temperature dimensional stability

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 - 1.16 g/cc1.10 - 1.16 g/cc
Density 0.0330 - 0.0350 g/cc0.00119 - 0.00126 lb/in³Free density, High Pressure Machine
 0.0340 - 0.0360 g/cc0.00123 - 0.00130 lb/in³Free density, Manual Mixing(low pressure machine)
 0.0600 - 0.0800 g/cc0.00217 - 0.00289 lb/in³Mold density; GB 6343
Viscosity 300 - 600 cP300 - 600 cPDynamic
Storage Temperature 10.0 - 25.0 °C50.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength >= 0.250 MPa>= 36.3 psiGB/T8813
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity <= 0.0330 W/m-K
@Temperature 15.0 °C
<= 0.229 BTU-in/hr-ft²-°F
@Temperature 59.0 °F
GB 3399
 
Processing PropertiesMetricEnglishComments
Cure Time >= 2.50 min>= 0.0417 hourTack free time, Manual mixing
 >= 2.50 min>= 0.0417 hourTack free time, High pressure machine
Gel Time 1.30 - 2.67 min1.30 - 2.67 minHigh Pressure Machine
 1.30 - 3.30 min1.30 - 3.30 minManual Mixing
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearanceLight yellow to brown transparent liquid
Closed-cell rate=90%GB 10799
Dimensional stability=1.0%24h, -30?; GB/T8811
 =1.5%24h, 100?; GB/T8811
Hydroxyl value250-450 mgKOH/g
Recommended Ratio1:1.40-1.1.60POL/ISO, Manual mixing
 1:1.40-1.60POL/ISO, High pressure machine
Rise time15-35 secHigh Pressure Machine
 20-40 secManual Mixing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM011 / 312540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.