MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chengdu Letain ZW-3100 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Resin of LTP ZW-3000 serials is crystal whisker reinforced materials with wear-resisting property based on high molecular weight linear PPS. Its characteristics are as following: (1)elevated temperature property:long run under 180-220 ?;(2)self-lubricating property:work for long time without any lubrication additive under usage Temperature: (3)resistance to solvent:not swelling in oil, organic solvent, especially in gasoline, diesel oil alcohols and aromatic series esters;(4)high thermal conduction:the heat by friction can transfer through metal parts or air when used under elevated temperature? As high strength and low density in one, Resin of LTP ZW-3000 serials are broadly applied as wear resisting parts under elevated temperature and humidity work conditions for aerospace, automotive, machine, household appliances, petroleum and chemical industry, such as bearing, axile bush, gear wheel, impeller blade, belt roller, brake block and so on.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 - 1.82 g/cc0.0549 - 0.0658 lb/in³GB1033
Water Absorption 0.20 - 0.40 %0.20 - 0.40 %GB1034
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in80×80×3.0
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in80×80×3.0
Melt Flow 20 - 120 g/10 min20 - 120 g/10 minGB3682
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 80 - 12080 - 120GB9342
Tensile Strength 100 MPa14500 psiGB/T1040
Elongation at Break 1.2 %1.2 %GB/T1040
Flexural Strength 120 MPa17400 psiGB1042
Compressive Strength 180 MPa26100 psiGB1041
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²GB/T1043
Coefficient of Friction 0.10 - 0.300.10 - 0.30kinetic
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 - 1.00e+13 ohm-cm1.00e+10 - 1.00e+13 ohm-cmGB/T1410
Surface Resistance 1.00e+10 - 1.00e+14 ohm1.00e+10 - 1.00e+14 ohmGTB/T1410
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 245 - 270 °C473 - 518 °FGB1634
Flammability, UL94 V-0V-0
 
Descriptive Properties
PV value800-1600
Tear and wear ratio0.1-0.002[mm3/Kg/Km], 45#

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT015 / 255868

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.