MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeoGraf GRAFCELL® GDB Graphite Gas Diffusion Barrier
Categories: Carbon; Graphite

Material Notes: GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductivity, and corrosion resistance. GDB material can be engineered to provide the liquid and vapor permeability characteristics that are required to achieve an optimum balance of oxidant and product. It can be used as a standalone component or in conjunction with a gas diffusion layer to passively regulate the balance of incoming air and product water. It enables a method of operation that reduces or eliminates the need for an actively controlled external balance of plant systems. It also enables simplified flow field plate designs. GrafTech manufactures diffusion barrier material as a continuous roll good with open areas of 3%-15% . GDB material is used in applications such as self humidified PEM fuel cell stacks and air cooled PEM fuel cell stacks. In self humidified PEM fuel cell stacks, GDB passively regulates the diffusion of product water from the cathode, keeping the polymer electrolyte membrane hydrated and maximizing proton conductivity without the need for an external humidification system. In air cooled PEM fuel cell stacks, GDB’s directional permeability and water retention characteristics enable the stack to be operated with air flow rates that are sufficient to cool the stack, eliminating the need for liquid coolant pumps and external radiators.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.300 - 1.60 g/cc0.0108 - 0.0578 lb/in³
Permeability 1.5 - 151.5 - 15sec/100cc; Gurley 4118 (100cc volume, 0.1 in² orifice); Air; Through-Plane
 10 - 10010 - 100cm³/(cm²*s); Gurley 4118 (100cc volume, 0.1 in² orifice); Air; Through-Plane
Thickness 130 - 160 microns5.12 - 6.30 milASTM-D645
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.500 - 1.00 MPa72.5 - 145 psiASTM-D828
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000400 ohm-cm0.00000200 - 0.00000400 ohm-cmIn-Plane; ASTM-C611
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity <= 214 W/m-K<= 1490 BTU-in/hr-ft²-°FIn-Plane; Angstrom's Method
 
Descriptive Properties
Area-Specific Electrical Resistance (mOhm·cm²)3 to 7ASTM-C611; Through-Plane
Basis Weight (g/m²)90ASTM-D646
Stiffness (Taber units)0.5-1.2Taber Model 150-E
Surface Contact Angle (degrees)90-130optical (Tantec Half-Angle™ Technique)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
NeoGraf eGRAF® SPREADERSHIELD™ SS1500 Graphite
NeoGraf eGRAF® SPREADERSHIELD™ SS400 Graphite
GrafTech A1 Acrylic Based Adhesive
GrafTech C1 Acrylic Coating

CGRAF925 / 107329

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.