MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® DC 4470 R PEEK, for Dental Use
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® DC4470 R is a gingiva-colored polyether ether ketone (PEEK) grade that is especially designed for removable dentures to meet the aesthetic demands of the patient.
Dry properties listed below
Industrial Sector: Medical Devices
Processing: Machining
Delivery form: Stock shape (rods and plates)
Optics: Opaque
Resistance to: Heat (thermal stability), Hydrolysis / hot water, Wear / abrasion, Fatigue resistance
Conformity: Biocompatibility, Medical application
Special Characteristics: Semi-crystalline
Regulatory: US Pharmacopeia Class VI conformity
Color: Gingiva-colored
Delivery form: Rods Ø6-20mm,stan.lengths 3000mm, Rods Ø70-100mm,stan.lengths 1000mm
Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oxidation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Water Absorption 0.400 %Sim to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 110 MPaISO 527
Elongation at Break 10.0 %ISO 527
Elongation at Yield 4.50 %ISO 527
Tensile Modulus 4400 MPaISO 527
Flexural Strength 170 MPaISO 178
Flexural Modulus 4400 MPaISO 178
Izod Impact, Notched (ISO) 5.40 kJ/m²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °CISO 75-1/-2
Vicat Softening Point 305 °C
@Load 5.10 kg
50 K/h; ISO 306
 335 °C
@Load 1.02 kg
50 K/h; ISO 306
 
Descriptive Properties
Color13.4Color b, CIE
 20.4Color a, CIE
 60.7Color L, CIE
 Gingiva-colored

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7859 / 324991

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.