MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Santoprene® 191-85PA Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft combinations are required. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

Key Features:

  • Designed for soft touch applications.
  • Designed for excellent adhesion onto nylon-6 (insert or 2K [two-shot] molding) and nylon 6,6 (2K molding only).
  • Adhesion values can vary according to type of nylon used, tool design and processing conditions.
  • EU and China RoHS compliant
Applications:
  • Automotive-Plugs, Bumpers, Grommets, Clips, Electronics, Kitchen Tools, Power Tools and Consumer Applications
Uses:
  • Appliance Components
  • Appliances
  • Automotive Applications
  • Automotive Under the Hood
  • Bonding
  • Cell Phones
  • Consumer Applications
  • Cookware Handles
  • Eyeglass Frames
  • Flexible Grips
  • Kitchenware
  • Living Hinges
  • Seals
  • Sporting Goods
  • Strain Reliefs
  • Tie-Layer
  • White Goods & Small Appliances
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282Air at 158°F, 168 hr; ASTM D573
 8282Air at 212°F, 168 hr; ASTM D573
 8383Air at 275°F, 168 hr; ASTM D573
 85
@Thickness 2.00 mm
85
@Thickness 0.0787 in
15 sec; ISO 868
Tensile Strength at Break 6.9141 MPa1002.8 psiAir at 275°F, 168 hr; ASTM D573
 7.4401 MPa1079.1 psiAir at 212°F, 168 hr; ASTM D573
 7.52 MPa1090 psiAcross Flow; ASTM D412
 7.7407 MPa1122.7 psiAir at 158°F, 168 hr; ASTM D573
Tensile Stress at Strain 4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 336.2 %336.2 %275°F, 168 hr; ASTM D573
 348.5 %348.5 %212°F, 168 hr; ASTM D573
 377.2 %377.2 %Air at 158°F, 168 hr; ASTM D573
 410 %410 %Across Flow; ASTM D412
Tear Strength 29.1 kN/m166 pli73°F, Die C; ASTM D624
Compression Set  27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 56 %
@Temperature 125 °C,
Time 252000 sec
56 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Descriptive Properties
ColorBlack
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer
ExxonMobil Santoprene® 191-70PA Thermoplastic Elastomer
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer
DSM Biomedical CarboSil® 40 90A Biocompatible Silicone Polycarbonate Urethane

PADVA088 / 22778

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.