MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 ISO Grade 32 CP Oil
Categories: Fluid; Lubricant

Material Notes: CP Oil is a low-viscosity, corrosion-preventive oil developed for the lubrication of air tools and other pneumatic equipment lubricated through air line lubricators, especially where the compressed air has high moisture content. CP Oil is formulated to provide excellent rust and corrosion protection and good wear protection for pneumatic tools, resulting in extended tool life. It has excellent metal-wetting ability to displace moisture from metal surfaces, and may be used as a rust preventive oil for metal parts stored indoors.

Applications:

  • Air tools and other pneumatic equipment lubricated through air line lubricators
  • Rust and corrosion-preventive oil for metal parts stored indoors
  • Lightly loaded plain and rolling-element bearings exposed to moisture
Features/Benefit:
  • Excellent rust and corrosion protection
  • Excellent metal-wetting ability
  • Good oiliness properties for wear protection
  • Does not form lacquer or gum on metal surfaces
  • Emulsifiable for easy removal from metal parts

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.865 g/cc0.865 g/cc
Density 0.863 g/cc0.0312 lb/in³
Viscosity Measurement 102102Index
Saybolt Viscosity at 100°F 166 SUS166 SUS
Saybolt Viscosity at 210°F 44.4 SUS44.4 SUS
Kinematic Viscosity at 40°C (104°F) 32.1 cSt32.1 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt5.4 cSt
ASTM Color 0.500.50ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0500.050[mg KOH/g]; ASTM D974
 
Thermal PropertiesMetricEnglishComments
Pour Point -27.0 °C-16.6 °F
Flash Point 233 °C451 °FCOC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON6025 / 210142

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.