MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

UNS C92800, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal and Sand.

Applications: Piston rings.

Classified under: Leaded tin bronzes

As cast values below are for sand casting. Alloy does not respond to heat treating

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.81 g/cc0.318 lb/in³Estimated
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8080
Tensile Strength, Ultimate 276 MPa40000 psias cast
Tensile Strength, Yield 207 MPa30000 psias cast
Elongation at Break 1.0 %1.0 %as cast
Tensile Modulus 110 GPa16000 ksi
Machinability 70 %70 %UNS C36000 (free-cutting brass) = 100%
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Melting Point 818.3 - 955.0 °C1505 - 1751 °F
Solidus 818.3 °C1505 °F
Liquidus 955.0 °C1751 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 79 %79 %
Lead, Pb 5.0 %5.0 %
Tin, Sn 16 %16 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UNS C90900, Copper Casting Alloy
UNS C90800, Copper Casting Alloy
Leaded Tin Bronze, UNS C92500, Copper Casting Alloy
Leaded Tin Bronze, UNS C92600, Copper Casting Alloy
Leaded Tin Bronze, UNS C92700, Copper Casting Alloy

MC92800b1 / 11943

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.