MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Sintox™ FA Mac-A95OR-1 Technical Ceramic
Categories: Ceramic

Material Notes: Alumina ceramic. This refractory-quality material is extensively used for high temperature applications in welding, heat treatment, and metallurgical and chemical processing.

Applications:

  • Welding nozzles
  • Stress relieving beads
  • Thermal insulators to protect workpieces during welding and heat treatment
  • Special crucibles for metallurgical and chemical processes.

    information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.70 g/cc0.134 lb/in³fired
Porosity 0.00 %0.00 %fully dense, nominal
Grain Size 6.0 µm6.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 45 N 7878
Hardness, Vickers 12.512.5Gpa @ Hv 0.5kg
Modulus of Elasticity 325 GPa47100 ksi
Flexural Strength 320 MPa46400 psi3 point; ASTM C1161
Compressive Strength 2000 MPa290000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.50 µm/m-°C
@Temperature 0.000 - 800 °C
4.17 µin/in-°F
@Temperature 32.0 - 1470 °F
Thermal Conductivity 21.0 W/m-K146 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 95 %95 %
 
Descriptive Properties
Colorpink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF8033 / 203510

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.