MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ResMart ABS VH-0815 BLK Flame retardant, Injection Molding
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: High flow, injection molding grade ABS with a UL94 5VA flammability rating

Information provided by ResMart

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Linear Mold Shrinkage 0.0034 - 0.0041 cm/cm0.0034 - 0.0041 in/inASTM D955
Melt Flow 3.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.8 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength at Break 27.6 MPa4000 psiASTM D638
Tensile Strength, Yield 39.3 MPa5700 psiASTM D638
Elongation at Break 17 %17 %ASTM D638
Tensile Modulus 2.00 GPa290 ksiASTM D638
Flexural Strength 58.6 MPa8500 psiASTM D790
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched 2.46 J/cm
@Thickness 6.35 mm
4.60 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.2 °C
@Thickness 6.35 mm
171 °F
@Thickness 0.250 in
ASTM D648
Vicat Softening Point 30.0 °C86.0 °FISO R306B
Flammability, UL94  V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 238 °C420 - 460 °F
Mold Temperature 37.8 - 82.2 °C100 - 180 °F
Drying Temperature 82.2 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 0.0689 - 0.138 MPa10.0 - 20.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRSMRT007 / 280645

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.