MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Maxlok™ T6 Acrylic Adhesive, with Lord Accelerator 4 Adhesive System
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: LORD Maxlok™ T6 acrylic adhesive when cured with LORD Accelerator 4 creates an adhesive system that will bond a wide variety of prepared or unprepared metals and plastics. LORD Maxlok T6 acrylic adhesive in combination with the recommended accelerator replaces welding, brazing, riveting and other mechanical fastening methods. LORD Accelerator 4 is a no-mix accelerator applied to the substrate before the acrylic adhesive.

Features: requires little or no substrate preparation. bonds a wide variety of substrates such as metals, ceramics and plastics. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility. performs at temperatures from -40 to +300°F (-40 to +149°C). resists dilute acids, alkalis, solvents, greases, oils and moisture; provides excellent resistance to indirect UV exposure, salt spray and weathering.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 - 1.07 g/cc0.0364 - 0.0385 lb/in³
Solids Content 100 %100 %after contact with LORD Accelerator 4
Brookfield Viscosity 80000 - 180000 cP
@Temperature 25.0 °C
80000 - 180000 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flash Point 15.0 °C59.0 °FClosed Cup
 
Processing PropertiesMetricEnglishComments
Pot Life 12.0 - 16.0 min
@Temperature 24.0 °C
12.0 - 16.0 min
@Temperature 75.2 °F
Time to Handling Strength
Shelf Life 6.00 Month
@Temperature 4.00 - 10.0 °C
6.00 Month
@Temperature 39.2 - 50.0 °F
in original, unopened container
 
Descriptive Properties
AppearanceOff-white to tan paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9109 / 232497

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.