MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Density 1.49 g/ccISO 1183
Filler Content 30 %
Moisture Absorption 0.060 %
@Temperature 23.0 °C
50%RH,23°C,24h; ASTM D570
Viscosity 110000 cP
@Shear Rate 3090 1/s,
Temperature 305 °C
ISO 11443
 138000 cP
@Shear Rate 3090 1/s,
Temperature 290 °C
ISO 11443
 157000 cP
@Shear Rate 1450 1/s,
Temperature 305 °C
ISO 11443
 172000 cP
@Shear Rate 3090 1/s,
Temperature 275 °C
ISO 11443
 215000 cP
@Shear Rate 1450 1/s,
Temperature 290 °C
ISO 11443
 218000 cP
@Shear Rate 681 1/s,
Temperature 305 °C
ISO 11443
 260000 cP
@Shear Rate 1450 1/s,
Temperature 275 °C
ISO 11443
 318000 cP
@Shear Rate 681 1/s,
Temperature 290 °C
ISO 11443
 322000 cP
@Shear Rate 316 1/s,
Temperature 305 °C
ISO 11443
 386000 cP
@Shear Rate 681 1/s,
Temperature 275 °C
ISO 11443
 454000 cP
@Shear Rate 316 1/s,
Temperature 290 °C
ISO 11443
 463000 cP
@Shear Rate 146 1/s,
Temperature 305 °C
ISO 11443
 560000 cP
@Shear Rate 316 1/s,
Temperature 275 °C
ISO 11443
 655000 cP
@Shear Rate 146 1/s,
Temperature 290 °C
ISO 11443
 663000 cP
@Shear Rate 73 1/s,
Temperature 305 °C
ISO 11443
 810000 cP
@Shear Rate 146 1/s,
Temperature 275 °C
ISO 11443
 935000 cP
@Shear Rate 73 1/s,
Temperature 290 °C
ISO 11443
 1.00e+6 cP
@Shear Rate 36 1/s,
Temperature 305 °C
ISO 11443
 1.17e+6 cP
@Shear Rate 73 1/s,
Temperature 275 °C
ISO 11443
 1.29e+6 cP
@Shear Rate 36 1/s,
Temperature 290 °C
ISO 11443
 1.62e+6 cP
@Shear Rate 36 1/s,
Temperature 275 °C
ISO 11443
 1.73e+6 cP
@Shear Rate 12 1/s,
Temperature 305 °C
ISO 11443
 1.97e+6 cP
@Shear Rate 7.3 1/s,
Temperature 305 °C
ISO 11443
 2.55e+6 cP
@Shear Rate 12 1/s,
Temperature 290 °C
ISO 11443
 2.96e+6 cP
@Shear Rate 12 1/s,
Temperature 275 °C
ISO 11443
 3.33e+6 cP
@Shear Rate 7.3 1/s,
Temperature 290 °C
ISO 11443
 4.11e+6 cP
@Shear Rate 7.3 1/s,
Temperature 275 °C
ISO 11443
Linear Mold Shrinkage 0.0063 cm/cm
@Thickness 1.60 mm
Transverse
 0.0075 cm/cm
@Thickness 3.20 mm
Transverse
Linear Mold Shrinkage, Flow 0.0035 cm/cmAnnealed; ISO 294-4
 0.0020 cm/cm
@Thickness 3.20 mm
 0.0021 cm/cm
@Thickness 1.60 mm
 0.0025 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0105 cm/cmAnnealed; ISO 294-4
 0.0085 cm/cm
@Thickness 2.00 mm
ISO 294-4
Melt Index of Compound 5.5 g/10 min
@Load 5.00 kg,
Temperature 280 °C
cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
 70ISO 2039/2
Hardness, Rockwell R 115ASTM D785
 115ISO 2039/2
Tensile Strength at Break 125 MPa
@Temperature 23.0 °C
ISO 527
Tensile Strength 55.2 MPa
@Temperature 150 °C
ASTM D638
 70.3 MPa
@Temperature 90.0 °C
ASTM D638
 126 MPa
@Temperature 23.0 °C
ASTM D638
 206 MPa
@Temperature -40.0 °C
ASTM D638
Elongation at Break 3.0 %
@Temperature -40.0 °C
ASTM D638
 3.3 %
@Temperature 23.0 °C
ASTM D638
 3.3 %
@Temperature 23.0 °C
ISO 527
 7.0 %
@Temperature 90.0 °C
ASTM D638
 7.5 %
@Temperature 150 °C
ASTM D638
Tensile Modulus 2700 MPa
@Temperature 150 °C
ASTM D638
 3280 MPa
@Temperature 90.0 °C
ASTM D638
 9300 MPa
@Temperature 23.0 °C
ISO 527
 9310 MPa
@Temperature 23.0 °C
ASTM D638
 9790 MPa
@Temperature -40.0 °C
ASTM D638
Flexural Strength 60.0 MPa
@Temperature 150 °C
ASTM D790
 86.2 MPa
@Temperature 90.0 °C
ASTM D790
 193 MPa
@Temperature 23.0 °C
ASTM D790
 266 MPa
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 2250 MPa
@Temperature 150 °C
ASTM D790
 2300 MPa
@Temperature 150 °C
ISO 178
 3000 MPa
@Temperature 93.0 °C
ISO 178
 3010 MPa
@Temperature 90.0 °C
ASTM D790
 7830 MPa
@Temperature 23.0 °C
ISO 178
 8280 MPa
@Temperature 23.0 °C
ASTM D790
 8900 MPa
@Temperature -40.0 °C
ASTM D790
 8900 MPa
@Temperature -40.0 °C
ISO 178
Compressive Strength 148 MPa
@Temperature 23.0 °C
ASTM D695
Izod Impact, Notched 101 J/m
@Temperature -40.0 °C
ASTM D256
 133 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 9.60 J/cm
@Temperature -40.0 °C
ASTM D4812
 9.60 J/cm
@Temperature 23.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 86.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
@Temperature 23.0 °C
ASTM D257
 1.00e+15 ohm-cm
@Temperature 23.0 °C
IEC 60093
Surface Resistance 1.00e+14 ohm
@Temperature 23.0 °C
ASTM D257
 1.00e+14 ohm
@Temperature 23.0 °C
IEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz,
Temperature 23.0 °C
ASTM D150
 3.3
@Frequency 1e+6 Hz,
Temperature 23.0 °C
IEC 60250
 3.4
@Frequency 1000 Hz,
Temperature 23.0 °C
ASTM D150
 4.2
@Frequency 100 Hz,
Temperature 23.0 °C
IEC 60250
Dielectric Strength 12.0 kV/mm
@Thickness 3.20 mm,
Temperature 150 °C
500 V/s, in oil; Short Time; ASTM D149
 14.5 kV/mm
@Thickness 1.60 mm,
Temperature 150 °C
500 V/s, in oil; Short Time; ASTM D149
 17.5 kV/mm
@Thickness 3.20 mm,
Temperature 95.0 °C
500 V/s, in oil; Short Time; ASTM D149
 21.5 kV/mm
@Thickness 3.20 mm,
Temperature 23.0 °C
500 V/s, in oil; Short Time; ASTM D149
 24.0 kV/mm
@Thickness 1.60 mm,
Temperature 95.0 °C
500 V/s, in oil; Short Time; ASTM D149
 26.5 kV/mm
@Thickness 1.60 mm,
Temperature 23.0 °C
500 V/s, in oil; Short Time; ASTM D149
Dissipation Factor 0.010
@Frequency 1000 Hz,
Temperature 23.0 °C
ASTM D150
 0.015
@Frequency 1e+6 Hz,
Temperature 23.0 °C
ASTM D150
 0.015
@Frequency 1e+6 Hz,
Temperature 23.0 °C
IEC 60250
Comparative Tracking Index 325 V
@Thickness 3.00 mm,
Temperature 23.0 °C
UL 746A
 
Thermal PropertiesOriginal ValueComments
Melting Point 250 °C10°C/min; ISO 11357-1/-3
 254 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 237 °CISO 75-1/-2
 240 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °CISO 75-1/-2
 220 °CASTM D648
UL RTI, Electrical 140 °C
@Thickness 0.750 mm
UL 746B
 140 °C
@Thickness 1.50 mm
UL 746B
 140 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical with Impact 140 °C
@Thickness 3.00 mm
UL 746B
 140 °C
@Thickness 1.50 mm
UL 746B
 140 °C
@Thickness 0.750 mm
UL 746B
UL RTI, Mechanical without Impact 140 °C
@Thickness 3.00 mm
UL 746B
 140 °C
@Thickness 0.750 mm
UL 746B
 140 °C
@Thickness 1.50 mm
UL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 3.00 mm
IEC 60695-11-10
 HB
@Thickness 0.750 mm
IEC 60695-11-10
 HB
@Thickness 0.750 mm
UL94
 HB
@Thickness 1.50 mm
UL94
 HB
@Thickness 3.00 mm
UL94
Oxygen Index 22 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °COptimum
 270 - 290 °C
Mold Temperature >= 95.0 °C
 110 °Coptimum
Drying Temperature 120 °C
Dry Time 4.00 hour
Moisture Content <= 0.020 %
 
Descriptive Properties
AdditiveImpact Modifier
AppearanceNatural Color
Drying RecommendedYes
FeaturesImpact Modified
 Impact Resistance, Good
 Stiffness, Good
 Strength, Good
 Thermal Aging Resistance, Good
FillerGlass fiber reinforcement
GenericPET
Heat StabilizedYes
Material StatusCurrent
Part Marking Code>PET-IGF30<ISO 11469
Polymer FamilyPolyester
Polymer TypePET
Processing MethodInjection Molding
Product CategoryGlass Reinforced Resins
 Toughened Resins
Resin IdentificationPET-IGF30ISO 1043
Ultrasonic WeldableYes
UsesAutomotive Applications
 Housings
 Structural Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Rynite® 530 NC010 PET-GF30
Eastman Aqua 18696 PET
Lotte Advanced Materials Infino® AE-2230 PC/PET, 20% MF
Lotte Advanced Materials Infino® ASF-9810F PBT/PET/MF
Celanese Rynite® 408 NC010 PET (With Extended Stress-Strain Tabular Data)

PZDSZ1225_a / 234775

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.