MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hippe PF WV 201 Wood veneer Reinforced Phenolic Resin - Sheet
Categories: Polymer; Thermoset; Phenolic

Material Notes: Cross plied. Used in mechanical applications. Good mechanical properties.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 - 1.40 g/cc1.30 - 1.40 g/ccIEC 1212-2 8.1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 60.0 MPa>= 8700 psiIEC 1212-2 5.7
Flexural Strength >= 100 MPa>= 14500 psiPerpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 14.0 GPa>= 2030 ksiIEC 1212-2 5.2
Compressive Strength >= 220 MPa>= 31900 psiPerpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 15.0 MPa>= 2180 psiParallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 5.90 kJ/m²>= 2.81 ft-lb/in²Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 1.00 J/cm²>= 4.76 ft-lb/in²Parallel to laminations; IEC 1212-2 5.5.2
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 100 V>= 100 VIEC 1212-2 6.4
 
Descriptive Properties
Thermal Endurance120 T.I.IEC 1212-2 7.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Douglas-fir Plywood
Plywood
PTS Tristar® PC-30GF 30% Glass Reinforced Polycarbonate With Release
PTS Tristar® PC-10GF-HC-V 10% Glass Fiber Polycarbonate
Avient Edgetek® PC-30GF/000 BLACK Polycarbonate (PC)

PHIPPE925 / 121929

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.