MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: All values may vary dependent on specific design and usage

Alumel® is a registered trade name of Hoskins Manufacturing.

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Key Words: ASTM E230
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.61 g/cc0.311 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 586 MPa85000 psiAnnealed
 1030 MPa150000 psiStress relieved
 1170 MPa170000 psiHard
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000294 ohm-cm0.0000294 ohm-cm3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 °C
6.67 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.523 J/g-°C
@Temperature 20.0 °C
0.125 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 29.7 W/m-K206 BTU-in/hr-ft²-°F
Melting Point 1260 °C2300 °F
Maximum Service Temperature, Air 1260 °C2300 °FOperating Temperature
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.0 %2.0 %
Manganese, Mn 2.0 %2.0 %
Nickel, Ni 95 %95 %
 
Descriptive Properties
MagneticStrong
Temperature Coefficient of Resistance0.00188 ohms/ohm-°C0-100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hoskins Manufacturing Chromel® Thermocouple Wire
Sandvik Cuprothal Thermocouple
Aremco Heat-Away™ 641-EV Thermally Conductive Grease, Silver Filled, for High Vacuum Systems
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Aluminum Titanium Nitride (AlTiN) PVD Coating

NHOS0 / 17350

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.