MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Innospec FLEXAREN® 18002 EVA-Copolymer
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: CAS Number: 24937-78-8

FLEXAREN® 18002 – high quality ethylene vinyl acetate copolymer with 18% content of vinyl acetate. Manufactured by high pressure tubular process. FLEXAREN® 18002 is more elastic than LDPE and compatible with a wide range of polymers. It can be processed with the same equipment.

Application:

  • Crosslinked foams
  • Flexible articles
  • Agricultural films
  • Thick films for automotive sound isolation
Properties:
  • Flexibility (especially at low temperatures)
  • High transparency
  • Good mechanical properties
  • Good filler absorption

Information provided by Innospec Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³DIN EN ISO 1183-1
Vinyl Acetate Content 18 %18 %FTIR
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ISO 868
Hardness, Shore D 3535ISO 868
Tensile Strength at Break 21.0 MPa3050 psiISO 527 (PK 1 BA)
Elongation at Break >= 750 %>= 750 %ISO 527 (PK 1 BA)
50% Modulus 3.80 MPa
@Strain 50 %
3.80 MPa
@Strain 50 %
ISO 527 (PK 1 BA)
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 64.0 °C147 °FISO 306 Method A
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 150 °C212 - 302 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell A-C® 405M EVA copolymer
Honeywell A-C® 400A EVA copolymer
ExxonMobil EXXELOR™ VA 1801 Maleic anhydride functionalized elastomeric ethylene copolymer
Honeywell A-C® 405T EVA copolymer
Innospec FLEXAREN® 14003 EVA-Copolymer

PINOS011 / 183454

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.