MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.

Available in: Asia Pacific and Europe

Product Applications: TECHNYL® B 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry; especially for the production of unpainted external parts due to its excellent surface finish, such as: door mirror housing, door handles. This product is available in grey and black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183/A
Water Absorption 0.95 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0070 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 185 MPaISO 527 Type 1A
Elongation at Break 3.0 %ISO 527 Type 1A
Tensile Modulus 9800 MPaISO 527 Type 1A
Flexural Modulus 8300 MPaISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 80.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohmIEC 60093
Dielectric Constant 3.7IEC 60250
Dielectric Strength 34.0 kV/mmIEC 60243
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 300 VSolution B; IEC 60112
 450 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 242 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 230 °CISO 75/Af
Oxygen Index 23 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Feed Temperature 255 - 265 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone260-270°C
Fire and smoke F index1NF F 16 101
Mixing Zone270-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY

PRHOD735 / 137966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.