MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubriplate Food Grade Cooker Oil USP Mineral -Based Food Machinery Grade
Categories: Fluid; Lubricant

Material Notes: This zinc free oil is designed for use in the Manzel Lubricators and Micro-valve systems found on most cookers and sterilizers used in canning operations and other similar applications involving high temperature and high humidity conditions. Unique additives provide high load-carrying ability and corrosion protection.

Available in Bottles, Jugs, Pails, 1/4 Drums and Drums

H-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.

Information provided by Lubriplate

Key Words: Part Number L0701-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 104104Viscosity Index
 150150ISO Grade
Saybolt Viscosity at 100°F 795 SUS795 SUS
Saybolt Viscosity at 210°F 82 SUS82 SUS
Kinematic Viscosity at 40°C (104°F) 155 cSt155 cSt
Kinematic Viscosity at 100°C (212°F) 16 cSt16 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Flammability Test 525525[°F] Fire Point
Flash Point 246 °C475 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
SAE Gear Oil No.90
SAE No.40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WLUBR164 / 76210

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.