MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Vitox® AMC Alumina Matrix Composite Technical Ceramic
Categories: Ceramic; Ceramic Matrix Composite

Material Notes: A very high purity, sub-micron grain sized zirconia toughened alumina matrix composite ceramic.

Applications:

  • Joint replacement components
  • Femoral heads to match cup liners of same material, HIP Vitox or UHMWPE
  • Cup liners
  • Other implantable devices

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.26 g/ccfired
Grain Size 0.16 µmaverage, Y-PSZ
 0.67 µmaverage, alumina
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 17Gpa, @Hv 1.0 Kg
Modulus of Elasticity 370 GPa
Flexural Strength 400 MPabiaxial
 700 MPa4-point
Fracture Toughness 4.50 MPa-m½SEVNB
 5.70 MPa-m½indentation
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Vitox® AMC Alumina Matrix Composite Aluminum Oxide Ceramic
Thermal Ceramics FireMaster Firecrete 85
Silicon Carbide, Reaction-Bonded, SiSiC
85% Alumina, vitreous body
Overview of materials for Stainless Steel

CMORF8020 / 203497

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.