MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinelec CCB2765 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Availability: Africa & Middle East; Latin America; Asia Pacific; South America

Features: Electrically Conductive

Uses: Sheets

Forms: Pellets

Processing Method: Injection Method; Sheet Extrusion; Vacuum Forming

Information Provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
Melt Flow  5.0 g/10 min
@Load 10.0 kg,
Temperature 200 °C
5.0 g/10 min
@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
 100 g/10 min
@Load 21.6 kg,
Temperature 200 °C
100 g/10 min
@Load 47.6 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Flexural Strength 28.0 MPa4060 psiASTM D790
Flexural Modulus 1.50 GPa218 ksiASTM D790
Izod Impact, Notched 1.12 J/cm
@Temperature 22.8 °C
2.10 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1e+051e+05ASTM D257
Surface Resistance 1e+051e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Edistir N 1910 Polystyrene
Versalis Edistir N 2982 Polystyrene
EMS-Grivory Grilamid® L 25 W 40 ESD PA12
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
Teijin Panlite® E-8715 EMS Shield Grade Polycarbonate

PTEKNP196 / 129277

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.