MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huber Martoxid® KMS-99 Calcined Aluminum Oxide
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Martoxid® KMS-99 calcined aluminum oxide is a high purity feedstock ready to press for uniaxial and isostatic pressing for the production of oxide ceramic bodies such as grinding media, insulating and wear-resistant parts, etc., produced in Bergheim, Germany.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.45 g/cc
@Pressure 100 MPa
2.45 g/cc
@Pressure 14500 psi
Pressed
 3.92 g/cc
@Treatment Temp. 1600 °C
3.92 g/cc
@Treatment Temp. 2910 °F
Sintered
Bulk Density 1.30 g/cc0.0470 lb/in³
Moisture Absorption <= 0.400 %<= 0.400 %
Particle Size 170 µm170 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 17 - 2017 - 20[kN/mm²], HV2, Sintered product
Modulus of Elasticity 380 GPa55100 ksi
Flexural Strength >= 330 MPa>= 47900 psi4-point Method, Sintered product
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.0 kV/mm889 kV/inSintered product
 
Thermal PropertiesMetricEnglishComments
Shrinkage 15.5 %15.5 %Upon sintering
 
Component Elements PropertiesMetricEnglishComments
Na2O 0.030 %0.030 %
 
Descriptive Properties
Al(OH)3>99%
FunctionalityReady-To-Press Granulating
Functionality: Mechanical hardnessWear Resistant Material
Market/Application: IndustrialCeramics

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER807 / 300913

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.