MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman DOM Plasticizer
Categories: Other Engineering Material

Material Notes: Product Description: Eastman™ DOM is a co-monomer normally used in polymerization with vinyl acetate, vinyl chloride, styrene and derivatives of acrylic and meth-acrylic acids. Eastman™ DOM is used as a specialty plasticizer and can be used in applications such as latex paints and textiles.

Application/Uses:

  • Coatings

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³
Viscosity 15 cP15 cP
Vapor Pressure <= 1.34e-7 bar<= 0.000100 torr
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.010<= 0.010
 
Thermal PropertiesMetricEnglishComments
Melting Point -76.0 °C-105 °FFreezing Point
Boiling Point 365 °C689 °F
Flash Point 185 °C365 °FSetaflash Closed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4531.453
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5220 / 222414

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.