MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PS 125 PS (Global)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: 125 is general purpose Polystyrene manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and high clarity. It also has medium vicat and heat deflection temperatures and makes it suitable for various applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³ASTM D1895
Density 1.05 g/cc
@Temperature 23.0 °C
0.0379 lb/in³
@Temperature 73.4 °F
Load Density; ASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 9595ASTM D785
Hardness, Rockwell M 6363Based on Injection molded specimens.; ASTM D785
Tensile Strength, Yield 43.0 MPa6240 psiASTM D638
Elongation at Yield 2.0 %2.0 %ASTM D638
Tensile Modulus 2.598 GPa376.8 ksiASTM D638
Flexural Strength 82.0 MPa11900 psiASTM D790
Flexural Modulus 3.529 GPa511.8 ksiASTM D790
Izod Impact, Notched 0.120 J/cm0.225 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FAnnealed; ASTM D648
Vicat Softening Point 98.0 °C208 °FRate A/50°C; ASTM D1525
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11599 / 245066

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.