MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast 50-3/AboCure 50-3 Clear Epoxy Adhesive and Casting Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 50-3 is a medium viscosity, clear Epoxy Resin. AboCure 50-3 is clear-amber in color, room-temperature-cure, and slow. It has variable ratios and low viscosity. AboCast 50-3/AboCure 50-3 is used for casting, potting, and encapsulating applications where bubble-free flow, high resistivity, and low exotherm are needed simultaneously.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.49 %
@Time 605000 sec
Viscosity 2500 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8600 psi
Elongation at Break 6.0 %
Compressive Strength 11300 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 72.0 °CDeflection Temp at unknown load
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Pot Life 180 min
 
Descriptive Properties
Hardening Time (min)720
Parts by Weight (pbw)100AboCast 50-3
 40AboCure 50-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboCast 10-5/AboCure 3-4 Epoxy
Abatron AboCast 10-5/AboCure 50-3 Epoxy
Abatron AboCast 10-5/AboCure 50-12 Epoxy
Solvay MR Film Fluoropolymer Film
Solvay FM® 10 Epoxy Syntactic Core

PABC815 / 107799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.