MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SACO AEI EXTINITY® 0201-171 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: EXTINITY® 0201-171 is a highly loaded, RoHS compliant, flame-retardant concentrate that can be used for a variety of applications including film, sheet, and extrusion coating. EXTINITY® 0201-171 has been designed to be used as a cost effective flame retardant for film products made with polyethylene resin systems. Films produced using EXTINITY® 0201-171 can be formulated to pass flammability requirements including the Boston Fire Department Test (BFD IX-1), NFPA-701, UL 94 VTM-0 and MVSS-302 automotive requirements. EXTINITY® 0201-171 does not contain DBDPO/DBDPE additives.

Recommended Applications:
Film: Blown, Cast
Extrusion: Tubing, Coating, Sheet

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.69 g/cc1.69 g/ccASTM D792
Melt Flow 3.0 - 6.0 g/10 min3.0 - 6.0 g/10 minASTM D1238 Condition E
Storage Temperature 4.44 - 26.7 °C40.0 - 80.0 °F
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 36 %36 %ASTM D2863
 
Descriptive Properties
FormNatural Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSACO029 / 249396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.