Sparkle Silver® 3346-ST is a medium, bright, non-leafing aluminum pigment with excellent hiding power. It has slightly more sparkle than Sparkle Silver® 3333-AR. It provides exceptional brightness, and is controlled for a low seed level. Applications: Automotive |