  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Carlson Nitronic® 33® Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: General Description

Nitronic 33 is a nitrogen-strengthened austenitic stainless steel that combines high yield strength with excellent toughness and ductility. It’s magnetic permeability remains very low after severe cold working and at cryogenic temperatures.

The alloy is superior to 304 stainless in at least five specific areas: (1) Yield strength in the annealed condition is approximately twice that of 304, (2) it has excellent strength and ductility at cryogenic temperatures, (3)has better stress corrosion cracking resistance than 304, (4) low magnetic permeability is retained at cryogenic temperatures and after severe cold working and, (5) resistance to wear and galling is superior to the standard austenitic stainless steels.

The corrosion resistance of Nitronic 33 is superior to 409 and, in general, is nearly equal to 304. In weak acid solutions, the corrosion resistance of Nitronic 33 approaches that of 304. In more aggressive media Nitronic 33 is somewhat less resistance than 304.

Nitronic 33 is markedly more resistant than 304 and 304L to stress corrosion cracking in hot chloride solutions at lower stress levels. At higher stress levels (approx. 50 ksi and above) they are equal. Like most stainless steels, Nitronic 33 is prone to pitting and crevice corrosion in seawater and other aggressive environments, and should not be used under these conditions unless cathodically protected.

Although Nitronic 33 is considerably stronger than the conventional austenitic stainless steels, the same fabricating equipment and techniques can generally be used.

Applications

  • Cryogenic Service – tanks valves, piping, flanges, and structural supports
  • Abrasion/Wear Resistance – screens, racks, and wear plates
  • Electrical (low magnetic permeability) – conduit shielding, MRI scanner supports, fittings, underground transmission risers and pipe and electronic support members
  • Marine – mine sweeper components and perming piers
  • Nuclear – spent fuel casks (internal supports)
  • Process Equipment – heat exchangers, pressure vessels and piping where 304 is borderline with respect to stress corrosion cracking.

Information provided by Carlson

Key Words: UNS S24000; ASTM XM-29
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 241<= 241
Hardness, Rockwell B <= 100<= 100
Tensile Strength at Break >= 689 MPa>= 100000 psi
 1140 MPa
@Temperature -73.3 °C
166000 psi
@Temperature -100 °F
 1580 MPa
@Temperature -196 °C
229000 psi
@Temperature -320 °F
Tensile Strength, Yield >= 379 MPa
@Strain 0.2 %
>= 55000 psi
@Strain 0.2 %
 717 MPa
@Strain 0.2 %,
Temperature -73.3 °C
104000 psi
@Strain 0.2 %,
Temperature -100 °F
 1217 MPa
@Strain 0.2 %,
Temperature -196 °C
176500 psi
@Strain 0.2 %,
Temperature -320 °F
Elongation at Break >= 40 %>= 40 %
 20 %
@Temperature -196 °C
20 %
@Temperature -320 °F
 60.5 %
@Temperature -73.3 °C
60.5 %
@Temperature -100 °F
Abrasion 4.354.35415 rpm; 16 lb load; 10,000 rev
 7.957.95105 rpm; 16 lb load; 10,000 rev
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000700 ohm-cm0.0000700 ohm-cm
Magnetic Permeability 1.00171.001777°F
 1.0016
@Temperature -196 °C
1.0016
@Temperature -320 °F
 1.002
@Temperature -73.3 °C
1.002
@Temperature -100 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.1 µm/m-°C
@Temperature 25.6 - 93.3 °C
8.93 µin/in-°F
@Temperature 78.0 - 200 °F
 17.4 µm/m-°C
@Temperature 25.6 - 316 °C
9.68 µin/in-°F
@Temperature 78.0 - 600 °F
 19.51 µm/m-°C
@Temperature 25.6 - 649 °C
10.84 µin/in-°F
@Temperature 78.0 - 1200 °F
 21.04 µm/m-°C
@Temperature 25.6 - 982 °C
11.69 µin/in-°F
@Temperature 78.0 - 1800 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.80 %<= 0.80 %
Chromium, Cr 17 - 19 %17 - 19 %
Iron, Fe 61.43 - 69.05 %61.43 - 69.05 %
Manganese, Mn 11.5 - 14.5 %11.5 - 14.5 %
Nickel, Ni 2.25 - 3.75 %2.25 - 3.75 %
Nitrogen, N 0.20 - 0.40 %0.20 - 0.40 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek Nitronic® 33 Austenitic Stainless Steel
Carlson Nitronic® 50® Austenitic Stainless Steel
Carlson Nitronic® 60® Austenitic Stainless Steel
Carlson Nitronic® 30® Austenitic Stainless Steel
AK Steel 305 Austenitic Stainless steel

NCARLSO07 / 15814

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.