MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 32 Transparent Cutting Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Transparent Cutting Oil is suited for mild to moderate machining that requires a nonstaining fluid to permit view of the work piece. It is recommended for light machining of ferrous and nonferrous metals, such as mild steel, brass, copper, aluminum and magnesium. It also can be used as a hydraulic fluid in machines in which the cutting oil and the hydraulic oil are drawn from a common sump.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 148 SUS148 SUS
Saybolt Viscosity at 210°F 44 SUS44 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt32 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt5.4 cSt
ASTM Color 0.500.50
 
Thermal PropertiesMetricEnglishComments
Pour Point -17.8 °C0.000 °F
Flash Point 216 °C420 °F
 
Descriptive Properties
Chlorine1.95 wt.%
Copper Corrosion1A
SulfurMax 0.01 wt.%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON193 / 75230

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.