MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Applications
Microthene MP564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. MP564189 is 16 mesh powder and is also available in pellet form Petrothene GA564189.

Regulatory Status
MP564189 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520.

Processing Techniques
Specific recommendations for processing MP564189 can only be made when the processing conditions, equipment and end use are known.

Key Words: FDA 21 CFR 177.1520.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D1505
Melt Flow 20 g/10 minASTM D1238
Spiral Flow 12.6 inEquistar
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57ASTM D2240
Tensile Strength at Break 1200 psi20 in/min; ASTM D638
Tensile Strength, Yield 2100 psi20 in/min; ASTM D638
Elongation at Yield 12 %20 in/min; ASTM D638
Flexural Modulus, 1% Secant 63000 psi0.5 in/min; ASTM D790
2% Secant Modulus 55000 psi0.5 in/min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °FASTM D648
Vicat Softening Point 196 °FASTM D1525
Brittleness Temperature <= -105 °FF50; ASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 350 °F
Middle Barrel Temperature 375 °F
Front Barrel Temperature 400 °F
Nozzle Temperature 400 °F
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
Total PPR Z9450 Random Copolymer Heat Sealable Grade

PEQU0852 / 157473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.