ATOFINA Propylene 13442 is a nucleated antistatic heterophasic copolymer. PPC 13442 is characterized by very high fluidity with good mechanical properties. It has been formulated for excellent antistatic properties.
ATOFINA Propylene PPC 13442 has been developed for high speed injection molding of thin walled packaging containers and household articles. Information provided provided by Total Petrochemicals. Total Petrochemicals acquired former Fina and Atofina plastics product lines. |