MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zinc Sulfide, ZnS, Sphalerite (Zincblende)
Categories: Ceramic; Sulfide/Chalcogenide; Other Engineering Material; Semiconductor

Key Words: Chalcogenide; Semiconductor
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.079 g/cc
a Lattice Constant 5.4093 Å
Formula Units/Cell (Z) 4
Molecular Weight 97.46 g/mol
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 1780N/mm²
Hardness, Mohs 3.8
Modulus of Elasticity 75.0 GPaCrystal structure not specified.
Flexural Strength 103 MPa4-pt. test; Crystal structure not specified.
Poissons Ratio 0.27Crystal structure not specified.
Shear Modulus 29.5 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -0.00000990Atomic (cgs)
Dielectric Constant 8.9
Band Gap 3.54 eV
Electron Mobility, cm²/V-s 180
Hole Mobility, cm²/V-s 5.0at 400°C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 390 J/gCrystal structure not specified.
CTE, linear 6.36 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.472 J/g-°C
Thermal Conductivity 25.1 W/m-K
Melting Point 1827 °CTransition at 1012°C
Heat of Formation 477 kJ/mol
Debye Temperature 257 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.356
IR Transmittance 72 %peak. absorption coefficient 0.1 at 8 µm/ 0.4 at 12 µm. Crystal structure not specified.
 
Descriptive Properties
CAS Number1314-98-3
ColorGray white
Crystal StructureCubicSphalerite Structure - Space Group F(-4)3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc Sulfide, ZnS, Wurtzite
Mateck Zinc Sulfide Cleartran (ZnS)
Mateck Zinc Sulphide, ZnS
Zinc Selenide, ZnSe
Schott IRC-1 Zinc Sulfide Broadband Infrared Ceramic

DSEN74 / 3083

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.