MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling GLASROD® Grade SG-200 Solid Rod and Bar
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Grade SG-200: Highest temperature – UL-rated for 210°C service. Grade SG-200 is a recognized component in UL listed Insulation systems for temperature rating of up to 200°C. Excellent thermal endurance. Ideal replacement for silicone rod. Available in Rectangular, Square “A” and Dogbones shapes. All GLASROD® solid rod and bar products features:
  • High physical strength
  • Excellent dielectric properties
  • Dimensional stability
  • Resistance to common solvents
  • Heat resistance
  • High strength-to-weight ration
  • Low water absorption
GLASROD® solid rod and bar products are fiberglass-reinforced thermoset polyester shapes which exhibit properties desirable for a wide range of structural and electrical applications. Superior strength provided by the continuous filament fiberglass roving is complemented by the physical and electrical characteristics contributed by the thermoset polyester resins. Together they provide the right combination of properties to offer significant price/performance advantages over alternative materials.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 483 MPa70100 psiASTM D638
Tensile Modulus 13.8 GPa2000 ksiASTM D638
Flexural Strength 552 MPa80000 psiASTM D790
Flexural Modulus 20.7 GPa3000 ksiASTM D790
Compressive Strength 96.5 MPa14000 psitransverse; ASTM D695
 345 MPa50000 psiaxial; ASTM D695
Izod Impact, Notched 21.4 J/cm40.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 6.40e+13 ohm6.40e+13 ohm
Dielectric Constant 5.0
@Frequency 60 Hz
5.0
@Frequency 60 Hz
Arc Resistance 150 sec150 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 µm/m-°C3.89 µin/in-°FASTM D696
Thermal Conductivity 0.288 W/m-K2.00 BTU-in/hr-ft²-°FASTM C177
Flammability, UL94 HBHB
Oxygen Index 21.8 %21.8 %ASTM D2863
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9375 / 233077

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.