MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Elantas EN-2555 (Conap) Potting and Encapsulation Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes:
Polyurethane Potting and Encapsulating Systems
Conathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many specific potting and encapsulating applications such as modules, strain-sensitive components, transformers, and coils. All 2500 series systems exhibit excellent performance when exposed to adverse environments and temperature ranges between -55°C and +130°C.

Cytec (Conap) EN-2555 Potting and Encapsulation Adhesive

  • Passes Thermal Shock Test (10 Cycles, -65°C to 130°C)
  • Non-Nutrient Fungus Resistance (MIL-STD-810B)
  • Mix Ratio: 24/100 (by Weight)

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³Cured
Water Absorption 0.40 %0.40 %24 hours
Water Absorption at Saturation 0.012 %0.012 %30 Days
Viscosity 600 cP
@Temperature 50.0 °C
600 cP
@Temperature 122 °F
Linear Mold Shrinkage >= 0.0060 cm/cm>= 0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Tensile Strength, Ultimate 13.8 MPa2000 psi
Elongation at Break 45 %45 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 7.70e+13 ohm-cm<= 7.70e+13 ohm-cm
Surface Resistance 7.20e+14 ohm7.20e+14 ohm
Dielectric Constant 4.85
@Frequency 1000 Hz
4.85
@Frequency 1000 Hz
Dielectric Strength 18.5 kV/mm
@Thickness 1.59 mm
471 kV/in
@Thickness 0.0625 in
Dissipation Factor 0.035
@Frequency 1000 Hz
0.035
@Frequency 1000 Hz
Arc Resistance >= 190 sec>= 190 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 114 µm/m-°C
@Temperature 20.0 °C
63.3 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.154 W/m-K1.06 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 100 °C
24.0 hour
@Temperature 212 °F
Full Cure in 24 hrs at 100°C
Pot Life 40.0 - 50.0 min
@Temperature 50.0 °C
40.0 - 50.0 min
@Temperature 122 °F
1 lbm
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCYTEC28 / 29260

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.